WIG welding wire 2.4627 welding electrodes NiCr22Co12Mo9 Nickel welding rods Ø0.8–5mm
Nickel-based alloy 2.4627 – heat-resistant welding filler material with high mechanical strength as well as good oxidation and corrosion resistance. Used for gas turbines, ethylene plants, and nickel-chromium-cobalt-molybdenum and nickel-iron-chromium alloys. Available from Auremo.
Length tolerance +/-2mm
Description:
Nickel-based alloy with high heat resistance combined with excellent mechanical strength. Material 2.4627 is a high-temperature alloy. These welding rods are used for welding nickel-chromium-cobalt-molybdenum alloys. Material 2.4627 can also be used for cladding overlays where a closely matching alloy is required, e.g. for gas turbines and ethylene plants.
The weld metal provides good strength and oxidation resistance from 800 to 1150 °C, especially when welding base metals made of nickel-iron-chromium alloys.
Please note the permissible operating temperatures for the filler metal and the base material: 2.4663, 2.4851, 1.4958, 1.4876. Inconel alloys 800HT and 803, and cast alloys such as HK-40, HP and HP-45 Modified.
Properties of material 2.4627:
- good durability
- resistance to deformation
- excellent corrosion resistance
Use of material 2.4627:
- high heat resistance
- excellent mechanical strength
- good strength and oxidation resistance
Main application of material 2.4627:
- gas turbines
- ethylene plants
- nickel-chromium-cobalt-molybdenum alloys
- nickel-iron-chromium alloys
If you would like to learn more about the possibilities of our online shop Auremo, we recommend taking a look at our range. With us, you will find not only electrodes, but also wires, sheets, bars and rare metals at attractive prices.
Technical data:
| Brand: | Auremo |
| Country and manufacturing region: | Germany |
| Manufacturer part number | Not applicable |
| Type: | Welding electrodes |
| Standard classifications: | |
| Material number: | 2.4627 |
| EN ISO 18274 | S Ni 6617 |
| AWS SFA-5.11 | ER NiCrMo - 1 |
Chemical composition (in %):
| C | Al | Cr | Co | Mo | Ni |
| 0.1 % | 1.2% | 22% | 12.5% | 9% | Balance |
Mechanical properties (room temperature):
| Tensile strength Rm MPa | Yield strength Rp 0.2 MPa | Charpy impact strength ISO-V J | Elongation at break A5% |
| 700 | 400 | 60 | 30 |