Welding wire WIG 2.4610 Alloy C4 welding rods hastelloy® C4 Ø2.4mm
Hastelloy 2.4610 – heat- and corrosion-resistant nickel-based alloy with high resistance to deformation as well as pitting, crevice, and surface corrosion. Used in the chemical industry, nuclear technology, turbine and aircraft construction. Available from Auremo.
Length tolerance +/-2mm
Description:
Hastelloy alloys that our online shop Auremo offers for purchase are heat-resistant corrosion-resistant materials. This is one of the most requested steels in the world, with the broadest application across industry.
Heat-resistant Hastelloy alloys contain nickel, chromium, vanadium, molybdenum, manganese, titanium, and aluminum, which determine the properties and parameters of the products based on them. This special alloy was originally developed to meet the needs of the chemical industry. It was intended to ensure the performance of pipeline parts and components at the highest temperatures and pressures.
At the same time, work was often carried out in aggressive environments and the transported materials were chemically active. The result is a qualitatively new Hastelloy alloy that offers maximum resistance to any type of corrosion (surface, crevice, pitting).
Material properties of grade 2.4610:
- good durability
- resistance to deformation
- excellent corrosion resistance
Use of material grade 2.4610:
- nuclear power industry
- manufacture of turbines
- aircraft construction
- chemical industry
Online shop Auremo offers only high-quality metals at affordable prices. If you have any questions, our customer service team will be happy to help you. In stock, there is always a wide selection of the highest-quality metals.
Technical data:
| Brand: | Auremo |
| Manufacturing country and region: | Germany |
| Manufacturer number | Not applicable |
| Type: | Welding electrodes |
| Standard classifications: | |
| Material number: | 2.4610 |
| EN: | NiMo16Cr16Ti |
| UNS | N06455 |
| Alloy | C-4 |
Chemical composition (in %):
| C | Si | Mn | Mo | Cr | Ni | Ti | Fe | Co |
| max. 0.015 % | 0.08% | 1.0% | 4.0-17.0% | 14.0-18.0% | balance | 0.7% | 3.0% | 2.0% |
Mechanical properties (room temperature):
| 0.2% proof strength Rp - N/mm2 | Tensile strength Rm N / mm² | Elongation A5% | Hardness HB 30 | Modulus of elasticity N/mm2 |
| 305 | 700 | 40 | 211 |
Physical properties (room temperature):
| Density in g/cm3 | Specific heat J/kg K | Thermal conductivity W/(mK) | Electrical resistance Ω·mm2/m |
| 8.6 | 408 | 10.1 | 1.24 |